Mike
I have not received any responce from Peter yet. I am looking forward to
his responce and secondly " e alternative to salt is vigilance and more
dross" What does vigilance mean is it a brand name? is this chemical
cause more dross? . As a responce to Mr. Sedlak we have been working
with alfachemicals but their stock is about to exhaust as far as I know.
Regards
Yusuf
Mike Fenner yazmış:
>I think you have your answer on the salts from Peter: If you buy a large
>amount to prevent being caught out again, just take care to keep it dry to
>prevent caking into lumps and spitting when you use it.
>
>
>
>Regards
>
>Mike Fenner
>Indium Corporation
>
>T: + 44 1908 580 400
>M: + 44 7810 526 317
>F: + 44 1908 580 411
>E: [log in to unmask]
>W: www.indium.com
>Pb-free: www.Pb-Free.com
>
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Baski Devre
>Sent: 13 July 2006 14:27
>To: [log in to unmask]
>Subject: Re: [TN] Roller Tinning Process
>
>Dear Sedlak and Mike
>Is it possible for you to give us more info about water soluble oil and
>do you have any brand that you will suggest us
>Best Regards
>
>Yusuf GÖMEÇ
>Product Quality Engineer
>
>
>BASKI DEVRE SAN ve TIC LTD STI
>Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
>Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
> 00 90 216 4836560 (4 Hat/Line)-173(Extention)
>Fax: 00 90 216 3544941
> 00 90 216 4913269
>Gsm: 00 90 533 6579897
> 00 90 533 7480014
>msn: [log in to unmask]
>
>
>
>R Sedlak yazmış:
>
>
>
>>Thanks for the explanation... I have heard/seen water soluble oil being
>>
>>
>used in roller tinning, and it apparently worked well.. have never heard of
>salt being used until now.
>
>
>> Rudy Sedlak
>>
>>Mike Fenner <[log in to unmask]> wrote:
>> The salt controls dross on the pot and (sometimes forgotten) ensures the
>>bottom roller remains tinned. The alternative to salt is vigilance and more
>>dross. Possibly you could use a [so called] water soluble oil, but I have
>>never seen this done, as these were introduced after roller tinning fell
>>
>>
>out
>
>
>>of use in Europe.
>>Roller tinning is an old process, but cheap. I think the nearest modern
>>equivalent process, to think of as an alternative, would be Hot Air Solder
>>Levelling. This would give much better or at least consistent solderability
>>and not have the blips on the trailing edge of pads.
>>
>>
>>Regards
>>
>>Mike Fenner
>>Indium Corporation
>>
>>T: + 44 1908 580 400
>>M: + 44 7810 526 317
>>F: + 44 1908 580 411
>>E: [log in to unmask]
>>W: www.indium.com
>>Pb-free: www.Pb-Free.com
>>
>>
>>
>>
>>-----Original Message-----
>>From: TechNet [mailto:[log in to unmask]] On Behalf Of Baski Devre
>>Sent: 12 July 2006 16:39
>>To: [log in to unmask]
>>Subject: [TN] Roller Tinning Process
>>
>>Dear Technetters
>>As you know that some PCB manufacturer uses roller tinning soldering
>>process. In this process firstly flux is spread over PCB and then passed
>>through rollers to be soldered. In this solder alloy sometimes a bit
>>salt is added to improve soldering quality and help solder to be appread
>>bright. I want to learn that if there is any alternative material used
>>in roller tinning soldering process to elaminate salt or is there any
>>alternative roller tinning soldering process flow.
>>Thanks in advance to your comments and knowledge share
>>Best Regards
>>
>>--
>>Yusuf GÖMEÇ
>>Product Quality Engineer
>>
>>
>>BASKI DEVRE SAN ve TIC LTD STI
>>Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
>>Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
>>00 90 216 4836560 (4 Hat/Line)-173(Extention)
>>Fax: 00 90 216 3544941
>>00 90 216 4913269
>>Gsm: 00 90 533 6579897
>>00 90 533 7480014
>>msn: [log in to unmask]
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>for additional information, or contact Keach Sasamori at [log in to unmask] or
>>847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>>
>>***This email, its content and any files transmitted with it are intended
>>
>>
>solely for the addressee(s) and may be legally privileged and/or
>confidential. If you are not the intended recipient please delete and
>contact the sender by return and delete the material from any computer. Any
>review, retransmission, dissemination or other use of, or taking of any
>action in reliance upon, this information by persons or entities other than
>the intended recipient is prohibited.
>
>
>>Messages sent via this medium may be subject to delays, non-delivery and
>>
>>
>unauthorized alteration. This email has been prepared using information
>believed by the author to be reliable and accurate, but Indium Corporation
>makes no warranty as to accuracy or completeness. In particular, Indium
>Corporation does not accept responsibility for changes made to this email
>after it was sent. Any opinions or recommendations expressed herein are
>solely those of the author. They may be subject to change without notice.***
>
>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>
>>
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>
>
>>To receive ONE mailing per day of all the posts: send e-mail to
>>
>>
>[log in to unmask]: SET Technet Digest
>
>
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>
>>
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>
>
>>-----------------------------------------------------
>>
>>
>>
>>---------------------------------
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>
>>
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>
>
>>To receive ONE mailing per day of all the posts: send e-mail to
>>
>>
>[log in to unmask]: SET Technet Digest
>
>
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>
>>
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>
>
>>-----------------------------------------------------
>>Talk is cheap. Use Yahoo! Messenger to make PC-to-Phone calls. Great rates
>>
>>
>starting at 1¢/min.
>
>
>>
>>
>>
>>
>
>
>
>
--
Yusuf GÖMEÇ
Product Quality Engineer
BASKI DEVRE SAN ve TIC LTD STI
Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
00 90 216 4836560 (4 Hat/Line)-173(Extention)
Fax: 00 90 216 3544941
00 90 216 4913269
Gsm: 00 90 533 6579897
00 90 533 7480014
msn: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|