Hi Tom,
We've been using Kleenox 'P' here for a couple of years now with great
success. I've tried other companies' products, but Kleenox is generally the
most effective - and with the least offensive fumes! Residue is not a
problem if you use the powder correctly - ie. use it sparingly, and give it
time to work. For a 800 Kg pot, a couple of tablespoons should be adequate
for each application.
We've also had good results running our pot at 240degreesC rather than 250.
Best Regards
Justin Braime
Production Engineering
Alpine Electronics of New Zealand Ltd
------------------------------------------------------------
15a Vestey Drive, Mt Wellington,
Private Bag 14921, Panmure,
Auckland, New Zealand.
Phone: +64-9-573 7100
Fax: +64-9-572 7101
-------------------------------------------------------------
----------
> From: Moss, Thomas <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Questions about KLEENOX "P"
> Date: Tuesday, 4 August 1998 08:28
>
> Hello all,
> I've been lurking on the list for awhile, but I thought I'd come
> out of hiding to ask some questions.
> I want to try some Kleenox "P" to reduce the amount of dross
> from our Wave Solder pot. Does anyone out there have any good or bad
> experiences with its use? Will its repeated use leave a residue or
> contamination in the solder? Are there any downsides that I'm not
> thinking of? Lastly, was it cost-effective for you to use?
>
> Thanks in Advance,
> Tom Moss
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|