TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wenger, George M.
Date:
Wed, 15 Jun 2005 17:32:44 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (89 lines)
Martin,

The use of nickel or ENIG is not necessarily a "no- no" for RF circuits.
If your RF products have long strip lines than your designers may not
want to use PCB traces that are plated with nickel.  When you start
using many small size discretes and fine pitch IC packages many people
have found that HASL is not a good choice.  From a soldering standpoint
ENIG or immersion silver should work fine.  Because of the brittle
solder joint failure that have been associated with ENIG we decided to
use immersion silver for all of our PCBs.  It has been a good choice for
us and we've not had any reliability issue since 1997.

Regards,
George
George M. Wenger, Andrew Corporation
Reliability / FMA Engineer
Base Station & Subsystems Group
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [log in to unmask]
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Martin Butcher
Sent: Wednesday, June 15, 2005 5:15 PM
To: [log in to unmask]
Subject: [TN] RF board finishes

Hi All,

We are currently assembling an RF product (first time build) that
utilizes
several fine pitch devices, leadless fine pitch devices and a great many
0402's.  The board finish is currently HASL and as the volume ramps up
there
is concern that defects related to the fine pitch and HASL will result
in
unacceptable costs.

We prefer to use ENIG as a surface finish for non-RF products that fit
this
Bill.  I seem to recall reading something on this very Net that
mentioned
nickel or ENIG being a no no for RF ccts.

I am not an RF guy and would love to get some feedback as to the effects
of
various board finishes on RF products.  Perhaps even recommendations as
to a
"good" finish that will give better yield than HASL.

Regards,
Martin Butcher,

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2