TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Nicolas van der Heyden <[log in to unmask]>
Date:
Tue, 26 May 1998 10:53:23 -0400
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Nicolas van der Heyden <[log in to unmask]>
Parts/Attachments:
text/plain (39 lines)
To All TechNeters,

SUBJETC: HASL alternative.

We are presently analysing some alternatives to HASL. We have some
questions about the OSP alternative.
What happens to the exposed copper for the following cases if the assembly
does not go through a wave process:

- Our products can require that the same PCB allows for variations.
Variations imply that the same PCB can call for all or only  components to
be assembled. When it is required to assemble a variation that excludes a
components, the stencil used in applying solder paste will "hide" the pads.
The OSP is pratically gone at the end of the process. This means that the
pads have no more protection again oxydation !

- What about the vias ?

Thanks in advance for your help.

                          ,,
                       ( . . )
----------o00---O---00o----------------------------------
         Nicolas van der Heyden

------------------------------------------------------------

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2