You can get fresh standardizing solution from any reputable Alpha Metals
distributor or rep.
Try Hisco, they have sales offices all over the U.S.
The standardizing solution is extremely critical to having an accurate
Omegameter, I would not attempt to deviate from the process as described
by Alpha.
If you are bringing back a Lazarus Omegameter, I would simply flush the
lines, clean the immersion tank, and replace the de-ionizing columns,
and re-calibrate using the resistor network provided with the machine.
http://www.hiscoinc.com/
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Skillborg, Fredrik
Sent: Wednesday, February 15, 2006 8:28 AM
To: [log in to unmask]
Subject: [TN] Resistivity calculator
Hello,
I am trying to bring life to an old Omega Meter but cannot get hold of
fresh Standardizing solution #3. Is there any calculator/table that
allows me to use some other concentration of the standardizing solution?
The nomgram from the manual only have a "calibration point" for the #3
solution.
Maybe this is a question that should have been put 25 years ago when the
equipment was new...
Thanks in advance.
// Fredrik
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|