TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Mon, 17 Dec 2001 14:10:10 -0000
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
From:
Mike Fenner <[log in to unmask]>
Parts/Attachments:
text/plain (86 lines)
A saponified wash is a particular sort of semi aqueous cleaning process.
"Saponify" means to turn into soap. So what happens when you use a
saponifier is that the resins in your flux residue are chemically turned
into soap, which is water soluble and can be rinsed off, also any greases,
oils that might be around. Which may or may no be desirable. This is as
opposed to simply being dissolved, or emulsified or whatever.

Saponifiers are also alkaline so will handily neutralise any acid residues.

Saponifiers need to be rinsed off thoroughly as being chemically active they
can cause corrosion just the same as fluxes, actually worse.

Not all no clean fluxes will saponify, and some not completely, so you will
need to check with your flux/paste suppliers.

You might need to check to see if there are any issues arising out of
machine discharges to the drain as well, your saponifier tech support people
can tell you where to start on that.


So far as cleaning no cleans are concerned, most people don't of course, but
it is a known and reasonably common procedure, you are not the first in
other words.


Best regards

Mike Fenner
Applications Engineer, European Operations
Indium Corporation
 T: + 44 1908 580 400
M: + 44 7810 526 317
 F: + 44 1908 580 411
 E: [log in to unmask]
W: www.indium.com
Leadfree: http://Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Marc Cowen
Sent: Monday, December 17, 2001 12:22 PM
To: [log in to unmask]
Subject: [TN] Saponified Wash


Hi All,

I am after some advice regarding saponified wash being used with a no-clean
process.
What is a saponified wash?
With regards to not using a wash with a no-clean process is it also common
practice to use this type of process flow (solder using no-clean flux then
through a saponified wash).

Thanks for your help.

Best regards

Marc Cowen.

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2