TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"d. terstegge" <[log in to unmask]>
Date:
Fri, 27 Oct 2000 15:09:58 +0100
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "d. terstegge" <[log in to unmask]>
Parts/Attachments:
text/plain (137 lines)
Hi,

It's been two weeks ago that I received some opinions about soldering of some 0.8 mm pitched BGA's with metal heatslugs on top (TI's partnumber TMX320C6203GLS). My final thought was that the risk of trying to shim these parts was higher than the risk of bridging, also considering the fact that the pad-design seemed decent. 
So we assembled those little monsters in the usual way, and hoped for the best. I just did an X-ray inspection and the BGA's looked perfect ! No squeezed balls, no bridges....

Oh, I want to thank everybody that adviced me in this! 

Kind regards,

Daan Terstegge
Unclassified mail
Personal Website: http://www.smtinfo.net

>>> "Rick Thompson" <[log in to unmask]> 10/10 3:37 pm >>>
Daan,

Based on our experience with the larger TI '6x' BGAs I'd agree with Ryan and
Steve.  With those parts we try to shim them so that ball collapse is 30-35%
of the ball diameter.

Rick Thompson
Ventura Electronics Assembly
2665A Park Center Dr.
Simi Valley, CA 93065

+1 (805) 584-9858 voice
+1 (805) 584-1529 fax
[log in to unmask] 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of d. terstegge
Sent: Tuesday, October 10, 2000 7:25 AM
To: [log in to unmask] 
Subject: Re: [TN] Heavy BGA's, now it's fine-pitch !


Hi Jim,

Thanks for the suggestion. Any idea on how thick such a spacer should be,
and how to apply it ?  Like I mentioned, trial and error is no option for
this project.

Kind regards,

Daan Terstegge
SMT Centre
Signaal Communications
Unclassified mail
Personal Website: http://www.smtinfo.net 

>>> "Marsico, James" <[log in to unmask]> 10/10 2:08 pm >>>
How about using a temporary spacer under each corner?

Jim M.


        -----Original Message-----
        From:   d. terstegge [SMTP:[log in to unmask]] 
        Sent:   Tuesday, October 10, 2000 9:59 AM
        To:     [log in to unmask] 
        Subject:        [TN] Heavy BGA's, now it's fine-pitch !

        Hi Technet,

        I need your advice on this one:
        Some time ago there was a discussion about soldering problems with
partnumberTMS320C6201GJC200 of Texas Instruments. It's a 1.27 mm pich BGA
with a heavy heat-slug on top. The weight of the heat-slug makes the
solderballs collapse a little too much, resulting in solder bridges.
        Now I've got to assemble some boards with similar parts, but with a
much smaller ballpitch of only 0.8 mm.
        No problem for the ordinary type BGA's, but with the heatsink I'm
starting to feel uncomfortable. For the record: it's TI's part
numberTMX320C6203GLS.
        I've got to build two boards, and all I've got is two components. No
trial and error possible......
        If anyone of you have experience or thoughts about this, please let
me know.

        Kind regards,

        Daan Terstegge
        SMT Centre
        Signaal Communications
        Unclassified mail
        Personal Website: http://www.smtinfo.net 




----------------------------------------------------------------------------
-----
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF TECHNET
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2