Hi Jim - I have used  impedance spectroscopy techniques to evaluate a
potential solder paste candidate and as a method of process control. The
test is very easy to conduct but you do need to have a good understanding
of how to generate a equivalent circuit model for the solder paste you are
testing and you do need to build up a use history to understand how the
modeling relates to manufacturing problems. The folks at ACI/EMPF in
Philadelphia are a good source of info (contact Greg Brobjorg at
610-362-1200, ext. 218 for more info on both the technique and equipment)
or shoot me an email with more specific questions. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]





Jim Kittel <[log in to unmask]> on 04/14/99 04:02:37 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to [log in to unmask]

To:   [log in to unmask]
cc:
Subject:  [TN] Impedance Measurements of Solder Paste




Technetters:
Is anyone using impedance measurement as a process control in their
manufacturing area?  I have a copy of a paper from the EMPF published in
the April/97 edition of 'Assembly' and it describes this process.  Looks
like an easy way to characterize paste.  Anybody using this technique to
identify bad paste?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2