TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Fri, 3 Mar 2000 12:27:50 +0100
MIME-Version:
1.0
X-To:
Brian Ellis <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Ingemar Hernefjord (EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (103 lines)
Aegreto Brianus, dum anima est, spes esse dicitur!
Not pig latin. Means approx "Said for Brian, a crazy person, but there is hope as long as there is life."
Acta est fabula, ergo plaudite et dulce perdidi.
.-- . / -- .- -.-- / .... .- ...- . / - --- / ..- ... . / .-.. .- - .. -. / .. -. / --- - .... . .-. / --.- .-. . --.- /
Over and out / Ingemar
Just had to do this, it's Fryday and soon time for both this and that. Yeaahooo!



Oh well! You asked for it, Ingemar, to misquote Virgil:
Ecce, igitur, hic canis non gelidus, Brianus, de montibus humor laborat.

Liberally translated for the non-Latin scholars this will give:
Lo and behold, therefore, this co-o-o-ol dog, Brian, tumbles down the mountains by way of a joke.
:-)

Brian

"Ingemar Hernefjord (EMW)" wrote:

> Couldn't resist teasing Brian. "vixi" means "stumbled". I guess Brian will give back with 200%. (more giggle) / Ingemar
>
> Subject: Re: [TN] How to detect contamination on metal surface
>
> Help me out Ingemar,
> My poor American education did not include Latin-what is "vixi"? I'm sure
> it's a very clever little joke.
>
> Timothy Reeves
> ECD Circuit Board Division
> 13626 South Freeman Road
> Mulino, OR 97042
> [log in to unmask]
> (503) 829-9108 (800) 228-8198  FAX (503) 829-5482
>
> > ----------
> > From:         Ingemar Hernefjord (EMW)
> > Sent:         Thursday, March 2, 2000 6:12
> > Subject:      Re: How to detect contamination on metal surface
> >
> > Veni vidi vixi (giggle, giggle)
> > Ingemar
> >
> >
> > Hi, all!
> >
> > OK, I may have been too categorical in my previous post. It may work for
> > some depending
> > on the degree of cleanliness they require, the purity of the water, the
> > substrate
> > material and the surface finish of the material under practical
> > conditions. I maintain
> > though that the basic premisses of the test are flawed and that universal
> > application
> > of it may lead to problems and disappointments - or worse.
> >
> > Caveat utilisator
> >
> > Brian
> >
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2