Tenison,
     The "OMIKRON" white tin is working great.  If you would like more
information on it, including references, you can contact me directly.


                                                                            St
ephen M. Wentz
                                                                            Fl
orida CirTech Inc.
                                                                            VM
# 408-233-0443

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2