TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Thu, 21 Mar 2013 15:29:09 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (37 lines)
I find semi-friendly ones easier to work with.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy
Sent: Thursday, March 21, 2013 7:57 AM
To: [log in to unmask]
Subject: Re: [TN] SAC 305 etch

To see Sn grain boundaries , don't etch.  Use cross-polarizers.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Thursday, March 21, 2013 10:53 AM
To: [log in to unmask]
Subject: [TN] SAC 305 etch

What would a good etch be for etching SAC305 solder joints to enhance viewing grain boundaries?

Thanks,
John

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2