If it is electrolytic nickel and flash gold we do not expect any tarnish in stored condition for at least 2 yrs.
Anil Kher
micro interconnexion pvt. ltd
D3-12A, Corlim Industrial Estate, Corlim , Ilhas , Goa - 403001
Tel: 0091-832-2284337 /209 , fax 2285271 / 2284209
Leaders in Gold Plated PCBs -Selective / COB
----- Original Message -----
From: Steve MacDonald
Sent: Tuesday, March 11, 2003 9:25 PM
Subject: Gold Tarnish.
Greetings Mighty Techneters.
Under normal environmental conditions, (As in no special effort is being made to create and maintian a particular controlled environment) how long will it take for Gold (gold fingers) to tarnish or show evidence of oxidation?
I am not considering any extremes in temperature and or humidiy. Just on a shelf at an assembly house.
I know how to clean them up, but someone asked me and I didn't have any range of responses to offer.
Thank you,
Steve M.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|