text/plain (65 lines)
We have been using a .018" (specified as .021" max.) in a .030 dia. pad for years and have not  had any problems.
Tom Burek


 -----Original Message-----
From: [log in to unmask] [SMTP:MIME :[log in to unmask]]
Sent: Thursday, February 03, 2000 11:29 PM
To: [log in to unmask]
Subject: [TN] VIA pads

 << File: ENVELOPE.TXT >>
 --------------------------------------------------------------------------  --
Good morning everyones around the World,

I have a design/manufacturing question.  If we use a 0,018" VIA, what is
the smallest pad size we can use on this VIA without causing problem in
PCB manufacturing?

thanks


Yvon Hache, P.Eng.
Tel: 506-863-2467
Email: [log in to unmask]

Concept + Inc.
Scientific Park, Suite 100
55 Crowley Farm Rd,
Moncton, NB
E1A 7R1

Tel: 506-858-4153
Fax: 506-858-4075
Web: www.concept-plus.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2