From: Dennis J Fall@TFT on 02/17/99 11:39 AM
To: [log in to unmask]
cc:
Subject: Plating solder onto isolated areas
I have been trying to find a way to plate solder onto isolated area on a
substrate. I need anywhere from 4-25 microns of solder covering copper
pads that are isolated from any other metal. So, electroplating may be
possible, but it is a matter of finding out how to do this. If there are
any ideas, please respond.
Thank You,
Dennis Fall P: 507-625-8445 x17
Engineer F: 507-625-3523
Thin Film Technology Corporation mailto:[log in to unmask]
1980 Commerce Drive http://www.thin-film.com
North Mankato, MN 56003-1702
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|