Anode- instead of only dissolution of copper ions there would be oxide
formation and perhaps oxygen evolution, and oxidation of organic addivites,
Cathode-hydrogen evolution, reduction of organic additive(depends on voltage
and nature of the additives), powdered metal deposits
Richard Haynes
609-497-4584
-----Original Message-----
From: Francis Lai <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Sunday, November 29, 1998 12:26 PM
Subject: [TN] What happens when polarising occurs
>I am just curious to know what would happen to the anode and the bath and
>
>the cathode when polarising i.e. drawing too much current from insufficient
>
>anode areas, occurs in an acid copper plating bath.
>
>My e-mail : [log in to unmask]
>
>Thanks to all of you in advance !!!!!
>
>Francis
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|