Guenter,
Thank you so much for the prompt reply.
Regards,
Wee Mei
Guenter Grossmann wrote:
> Wee Mei
>
> The question of design rules came up by the fact that the wetting
> behaviour of led free solder in the possible process window is somewhat
> different from the one of SnPb. However, our trials in LEADFREE and some
> pilot production in the companies associated in the project with
> standard design rules showed no problems in the soldering process due to
> the design. It can be, in wave soldering, if space is very restricted
> and thus no solder thieves can be used when soldering fine pitch
> components and components are set close together, you see more bridges .
> But it has to be emphasised that, if the IPC design rules are
> consequently applied, lead free soldering is not a big deal.
>
> Best regards
>
> Guenter
>
> EMPA
> Swiss Federal Institute for Materials Testing and Research
> Centre for Reliability
> Guenter Grossmann, Senior Engineer
>
> 8600 Duebendorf
> Switzerland
>
> Phone: xx41 1 823 4279
> Fax : xx41 1823 4054
> mail: [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|