On  4 Apr 98 at 15:03, John L. Schmalzel wrote:
> I am interested in expanding/upgrading our rapid prototyping PCB
> facilities at our University.  Currently, we have a T-Tech "Quick
> Circuit" CNC mill; however, we are interested in exploring other
> options.  Can you point us in the right direction to find similar
> rapid prototyping technologies?

Check out this Web Site: http://www.lpkf.de. This is the leading
company for PCB Prototyping equipment here in Germany LPKF Laser &
Electronics GmbH, but I think, they have a susidiary in USA, too.
They offer CNC mills with the option to get plated trough holes
without galvanic treatment and to get solder mask without
photoplotting.

mfg Matthias Mansfeld
-----------------------------------------------
Matthias Mansfeld Elektronik
* Printed Circuit Board Design and Assembly
Am Langhoelzl 11, D-85540 Haar, GERMANY
P.O.B. 1143, D-85529 Haar, GERMANY
Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
E-Mail: [log in to unmask]
Internet: http://home.t-online.de/home/matthias.mansfeld

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2