TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Vickie Chapman <[log in to unmask]>
Reply To:
Date:
Fri, 11 Jul 1997 10:02:39 -0700
Content-Type:
TEXT/PLAIN
Parts/Attachments:
TEXT/PLAIN (36 lines)

On Fri, 11 Jul 1997 06:16:37 -0700 [log in to unmask] wrote:

> From: [log in to unmask]> Date: Fri, 11 Jul 1997 06:16:37 -0700
> Subject: Re: Test and Inspection Strategy
> To: [log in to unmask]
> 
> Hi Vikcha and Thomas,
> Most likely the lack of responses comes from the large number of questions to
> which there are no real good clear cut answers. 

{some other interesting comments deleted}

OK, I'll generalize my question a bit more:

I am interested in talking to anyone who has any sort of experience, good or 
bad, with any automated equipment for inspecting solder joints on PCA's. 
Optical, laser, Xray, or other....

Thanks,

-- Vickie Chapman



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2