Check radiation hardening device on the web. The fine pitch device is
more sensitive to radiation damage (one single cascade zone will damage
few device... If the high energy beam is used). By the way, why you
need to zap with X-ray? Poor process development work? Lousy design?
Development should be done using dummy or others... I do not see a need
to zap production parts with high energy X-ray.... Must be something
new...
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of
>[log in to unmask]
>Sent: Thursday, May 29, 2003 9:09 PM
>To: [log in to unmask]
>Subject: Re: [TN] X-ray beam damaging flash memories
>
>
>Hi, Eric,
>
>I haven't experiences it, but I've certainly heard about it
>from the company that makes the X-Ray machinery we use. They
>did say that (with their equipment) exposure would have to be
>quite prolonged to cause the problem though. They did at least
>warn us when we asked the question about X-Ray hardening or
>other damage.
>
>Peter
>
>
>
>Eric Castonguay <[log in to unmask]> 29/05/2003 08:03 PM
>Sent by: TechNet <[log in to unmask]>
>
>Please respond to "TechNet E-Mail Forum."; Please respond to
>Eric Castonguay
>
> To: [log in to unmask]
> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
> Subject: [TN] X-ray beam damaging flash memories
>
>
>
>
>
>
>
>
>Hi guys,
>Never heard about this one in 4 years in the telecom industry.
>Our current supplier of flash memories found a very
>interesting reason why we are having problems with their
>parts. The strength of X-ray being used by the CM on our cards
>for 5-dx analysis is too strong, they said. Industry standard
>is 1K rad max I was told. Going above it causes issues with
>the analog section of the programming in the die.
>
>There were able to tweak the registers & re-test them and had
>no problems with the chips. They also tried re-exposing them
>and suceeded in repeating the problem. I asked if we could do
>anything to fix boards that have already been x-rayed and they
>said that this cannot be done once the parts are assembled on
>the boards.
>
>Considering that Flash is not the only component with an
>analog section in it, I think that it would be a good idea to
>investigate the x-ray equipment, strength & techniques at our
>CM, even if they use a standard Agilent 5DX machine. But first
>I want to hear if some of you ever met this problem before.
>
>Thanks.
>Eric
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not
the intended recipient, please delete it and notify us immediately; you
should not copy or use it for any purpose, nor disclose its contents to
any other person. Thank you.]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|