How do you cure the urethane"? Is it possible that the outside is curing
before the rest and what you are looking at is shrinkage voiding due to
the z axis depth?
John
John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kelly Morris
Sent: Tuesday, January 24, 2006 10:23 AM
To: [log in to unmask]
Subject: Re: [TN] Conforma Coat (Urethane) & bubbles
Steve has put my pictures on his web page. (THANK YOU STEVE!) The
pictures
are after conformal coat touch up, but they give an idea of the
location,
shape, etc.
They are at:
http://stevezeva.homestead.com/files/Conformal_Coat_Bubble.JPG
http://stevezeva.homestead.com/files/Conformal_Coat_Bubble_2.JPG
On Tue, 24 Jan 2006 09:25:25 -0600, Kelly Morris <[log in to unmask]>
wrote:
>We've got a problem here, where we're hand spraying a urethane
conformal
>coat on over a rectangular inductor.
>The inductor body is a plastic tube, with potting to fill.
>The top is not always flat (sometimes concave).
>The problem is that bubbles appear in the conformal coat on the potted
>surface, sometimes right after bake and sometimes days after.
>
>Any ideas on what the root cause is and how to prevent the bubbles?
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|