TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0ur3En-0000LBC; Thu, 15 Aug 96 09:17 CDT
Old-Return-Path:
Date:
Thu, 15 Aug 1996 10:14:46 -0500
Precedence:
list
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/5783
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Thu Aug 15 13:
27:30 1996
Resent-Message-ID:
<"Cjpio2.0.CkL.u5p4o"@ipc>
Subject:
From:
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (32 lines)

     
     I am working with a high-temp (> +175degC) soldering process which 
     requires that the plating and or coatings be removed/stripped from 
     component leads. This leaves the base metal (copper) exposed and then 
     we "tin" using production solder (high Pb-based alloy) to within one 
     lead diameter of the component body. (Don't want to expose the 
     component body to the molten solder within the solder pot due to 
     thermal shock and/or fatigue to component).
     
     Here's the question:
     
     1) What effects (corrosion, etc.) would we see if we left the 
     component lead base metal (copper) exposed at extended high temp with 
     the potential of moisture present ? 
     
     Any papers, and or technical resources avalibale that may address this 
     issue ?
     
     Thanks,
     
     D.Drake

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2