TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 15 Mar 2007 07:46:51 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Barmuta, Michael" <[log in to unmask]>
Subject:
From:
"Barmuta, Michael" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (147 lines)
Hi Steve: Seems like are getting a lot of replies but not much regarding
your actual question. Let me give you the short answer.

All plating is porous including nickel. Think of a sponge. Depending on
the type of plating chemistry and additives used this can be minimized
by creating denser less porous deposits. 

The thin nickel plating  will not be thick or dense enough to prevent
the copper from migrating or diffusing up thru the nickel and into the
gold. 


	
Regards
	
Michael Barmuta
	
Staff Engineer
	
Fluke Corp.
	
Everett WA
	
425-446-6076



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Thursday, March 15, 2007 4:32 AM
To: [log in to unmask]
Subject: Re: [TN] IPC ENIG SPECIFICATION

Thanks for the prompt reply. I can do the gold calculations - lots of
stuff on the tech-net telling me how to do that. We have not seen any
solderability issues. I would still like an explanation of the reasoning
behind the minimum nickel thickness( besides a keypad type application).
Regards Steve Kelly>

Steve,
>
> I will likely solder quite well, but the gold is quite thick for
> soldering to without incurring the wrath of gold embrittlement.  I
would
> not be so concerned about the thin nickel as the overabundance of
gold.
>
> If the gold were nice and soft, it would be nice for gold ball
bonding!
> But, the nickel is quite thin.
>
> If the numbers are correct, you did not receive ENIG - have them sent
> back
>
> Steve C
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
> Sent: Wednesday, March 14, 2007 9:31 PM
> To: [log in to unmask]
> Subject: [TN] IPC ENIG SPECIFICATION
>
> Hi All,
> I  have a question about this specification. Obviously when the
> technical
> gurus wrote this they had good reasons for specifying the nickel at a
> minimum of 118 microinches. One of our customers recently received
some
> parts from the far east. The print called for ENIG but the parts came
in
> with approx. 20 microinches of nickel and approx. 40 microinches of
> gold.
> My question is what are the reliability/solderability concerns on low
> nickel. Thanks in advance. Regards Steve Kelly
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
> ext.2815
> -----------------------------------------------------
>
> THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS
SENT
> FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED
ONLY
> FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you
are
> not the intended recipient, you are hereby notified that any review,
> distribution, or copying of this communication is strictly prohibited.
If
> you have received this communication in error, please immediately
notify
> the sender by return e-mail, and delete this e-mail message and any
> attachments from your computer.
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

This message (including any attachments) contains confidential 
and/or proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on 
the contents of this information is strictly prohibited and may 
constitute a violation of law.  If you are not the intended 
recipient, please notify the sender immediately by responding to 
this e-mail, and delete the message from your system.  If you 
have any questions about this e-mail please notify the sender 
immediately. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2