Are you referring to a board supplier or component supplier ?- all board
suppliers can provide lead free finishes today - Immersion tin, Enig,
immersion silver and OSP -that will solder with ordinary tin lead solder
alloy and with the lead free solders
Dougal Stewart
email: [log in to unmask]
phone: +44 1896 822204
mob: +44 7984 629667
----- Original Message -----
From: "Atkinson, Neil" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 14, 2002 5:22 PM
Subject: [TN] lead Free
> One of our suppliers is 'proposing' a new lead free finish which he says
> will solder perfectly well with 'normal' SnPb solder as well as Lead Free.
>
> The finishes they are proposing are SnAg, SnBi and SnCuAg. my question
is,
> Does anyone have experience with using these finishes through a normal
> process and are there any 'pitfalls' top look out for.
>
> There is a lot of talk about total Pb free processes but what about the
> interim - are the new finishes 'backwards compatible'!!
>
> Thanks in anticipation of everyone's responses.
>
> Neil
>
>
>
>
>
>
> ________________________________________________________________________
> This e-mail has been scanned for all viruses by Star Internet. The
> service is powered by MessageLabs. For more information on a proactive
> anti-virus service working around the clock, around the globe, visit:
> http://www.star.net.uk
> ________________________________________________________________________
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|