I am looking at some single sided boards that were assembled and soldered at
two different companies. Under magnification, the solder fillets to the
leads inside the holes (not the solder fillets on the solder side of the
board) have a characteristic that appears to be a defect. At the tops of
the fillets, which are generally shaped properly, there is a tiny gap,
usually around the entire circumference of the lead where the fillets appear
to have peeled away from the leads. Nearly all leads on each board exhibit
this characteristic.
The solder fillets on the solder side appear generally perfect.
Is this common to single sided boards? What is the cause and how can it be
corrected?
David North
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|