TECHNET Archives

June 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Date:
Mon, 8 Jun 2015 16:48:31 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Message-ID:
Subject:
From:
Richard Kraszewski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
I agree with Mike.  Biggest concern is a significant drop in activity.   Coalescence of the solder paste  into a single large ball when reflowed  on a  non-solderable  surface such as  a ceramic plate would  be a good start. One nice solder ball is what you're looking  for with minor if any adjacent solder fines not coalesced into  the large single ball.  If it looks good, I would still only keep it for about 25 % of its stated shelf life. 

Rich  Kraszewski /Plexus 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Friday, June 05, 2015 12:06 PM
To: [log in to unmask]
Subject: [TN] Solder Paste Question

Everyone,

We just received 25 tubes of solder paste that got misplaced by the carrier and was delivered in 6 days instead of the usual two.  When it arrived it was warm to the touch.

We performed a viscosity test after allowing it to stabilize to ambient, and the readings returned were within spec and very close to our typical results.

Is there any danger in using this shipment?

Thanks for your help!

Leland

________________________________

“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2