TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Blair K. Hogg" <[log in to unmask]>
Date:
Thu, 26 Feb 2004 12:58:28 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (123 lines)
        Steve:
        Take the inverse of the  Siemens reading and that will be in mega
ohms. Good DI water should be about 16 mega ohms or about 0.07 micro
siemens.
        Regards,
        Ramon

> -----Original Message-----
> From: Blair K. Hogg [SMTP:[log in to unmask]]
> Sent: Thursday, February 26, 2004 2:11 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Conductivity and Resistivity Correlation
> 
> Steve,
> 
> Conductivity in Siemens or Mhos is the reciprocal of Resistivity on Ohms.
1 uS conductivity is equal to 1 Mohm resistivity, 2uS is equal to 500kOhm,
etc.
> 
> Blair
> 
> 
> >>> [log in to unmask] 02/26/04 01:35PM >>>
> Hi All!
> 
> Is there any chart, formula, or conversion that I can use to correlate a 
> conductivity reading to a resistivity reading?
> 
> The reason I'm asking is that I have a new batch cleaner that has been up
and 
> running the last three weeks or so. One of the neat things with the
cleaner is that during the rinse cycle, it monitors the rinse water
resistivity to a 
> setting that you program in the machine. If it reaches that pre-programmed
resistivity setpoint before completing the number of rinse cycles that you
program, 
> it will terminate the rinse cycles and go into the dry cycle. If it never
reaches the resistivity setpoint within the number of rinse cycles that
you've 
> programmed, it will display "FAILED" on the touch screen. You can then run
another cycle, or start trying to figure out why the boards didn't come
clean.
> 
> Well, everything has been going fine with the cleaner up until yesterday.
Every batch of boards I ran failed the resistivity setting I had in the
machine. 
> 
> The manual recommends a setting between 350-750 kohms, I've had my setting
at 
> 550 kohms from the beginning, and everything has been fine. I've had to
lower 
> the setting to 400 kohms so the batches would pass. It's still within the
350-750 kohm range, but I'm curious why all of a sudden things won't pass at
550 
> kohm like it's been doing the few weeks.
> 
> So I called tech support for the cleaner, and they feel that my input DI 
> water may be going bad. I have a US Filters reverse osmosis filtering
system that 
> dumps that water into Ion exchange columns and that water goes directly to
my 
> cleaner. The DI system displays the conductivity of the output water in µS

> (micro-siemins). I want to correlate that to resistivity to see if my DI
water is 
> truly going bad.
> 
> Thanks!
> 
> -Steve Gregory-
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
> 
> 
> **********************************************************************
> This email and any files transmitted with it are confidential and
> intended solely for the use of the individual or entity to whom they
> are addressed. If you have received this email in error please notify
> the system manager.
> 
> This footnote also confirms that this email message has been swept
> for the presence of computer viruses.
> 
> www.hubbell.com - Hubbell Incorporated
> **********************************************************************
> 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e> 
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2