I haven't played with too many Fe etches but 2 to 5% HNO3 with the remainder ethyl alcohol does ok for low-mid carbon steels. Let the sample soak in solution for a minute or two.
Regards,
Andy
Andrew C. Giamis
Andrew Solutions
FMA / Reliability Engineer
40 Technology Drive,
Warren, NJ 07059
(908) 546-4686 [Office]
(908) 938-7945 [Cell]
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Friday, February 03, 2012 10:17 AM
To: [log in to unmask]
Subject: [TN] ASTM 4130 steel
Fellow TechNetters:
Can someone make a recommendation on the chemical etchant for the above mentioned steel. I am award that compatible material to this exists out there.
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|