TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Fri, 15 Sep 2006 17:12:36 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (68 lines)
Rick

I have never seen the variations in Dk you are describing. Something is
obviously going on. Does the supplier concur that this is the case? If so
what is their explanation.

 On the positive side, most electrical parameters vary with the square root
of Dk so a variation of 1.3 has the effect of 1.14 impact on most
performance parameters. Thank nature for small favors.

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389


----- Original Message -----
From: "Smith, Richard" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, September 15, 2006 11:46 AM
Subject: [TN] Laminate Material DK


I've seen differences of as much as 30% between a laminate manufacturer's
specified DK value and the board fabricators "effective DK" value for the
same material (FR4). Often the disparity is well outside of the range
specified by the material manufacturer. I understand that DK values can
change due to resin/content and frequency however, a 30% difference just
seems awful big.

Here's the part where I seek help from the experts. Thanks!

Is 30% difference in manufacturer DK versus Effective DK really possible?

Assuming the same material, will the DK difference be the same from
fabricator to fabricator?

Thanks Much!

Rick

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2