TECHNET Archives

June 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 27 Jun 2007 08:36:42 -0400
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Baine <[log in to unmask]>
Content-type:
text/plain; charset=iso-8859-1
Subject:
From:
Paul Baine <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (24 lines)
Hello all,

We are building a PWB Assy made up of both Rigid and Flexible PWB components.  We do not have much experience dealing with the Flexible part;  this Assy is a Customer design.

When we dealt strictly with Rigid PWB Assy's, we tested cleanliness using the ROSE (Resistivity of Solvent Extract) method, where a solution of alcohol and distilled water was sprayed over the PWB and the resistivity of the resulting solution was measured.

Our Manufacturing Manager does not want to spray any solution containing water over the Flex PWB section of the Assy because he is afraid that the Flex PWB layers may separate.  There is some evidence that he may be right.

Does anyone have any experience with cleanliness test for Rigid Flex PWB Assy's?  There are no components on the Flex part of the Assy - it is used as a "ribbon cable".

Paul Baine
Q.A. Manager
C-Tech Ltd.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2