Theoretically no, if it was properly applied in the first place. Provisos:
a) tender coatings, such as acrylics, like neither high temps nor
aggressive chemicals in your wash water.
b) silicone coatings will wash OK but you may have problems with
moisture absorption/adsorption in the drying stage.
c) urethanes and flexibilised epoxies should normally be OK
Brian
Ioan Tempea wrote:
> Dear Technos,
>
>
>
> A quick one : can I water wash conformally coated boards?
>
>
>
> This means conformally coated boards have been returned for rework, we
> will change the components (have to use WS flux) and have to wash.
>
>
>
> Can regular water wash at 140F do any damage to coating?
>
>
>
> Thanks,
>
>
>
> Ioan
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|