Ofer,
I would be very cautious using ENIG for the 60A circuit.
Even .1 ohm could cause an explosion (P = I2R = 360 Watts)!!
Use electrolytic gold for this one!
David A. Douthit
Manager
LoCan LLC
Ofer Cohen wrote:
>Techneters,
>I have to decide on a lead-free coating for a PCB. My natural tendency (based on previous experience) is to use immersion tin. There is one major issue - the PCB surface is in contact with bronze surface for safety grounding. How will the immersion tin behave along time?
>
>In another instance I selected ENIG, because the surface contact is used as a power conductor, and will conduct continuously 60A on an area of 220 square mm (~.35 square "). Will the surface contact withstand this current? Is gold plating better for this application?
>
>Regards
>Ofer Cohen
>Seabridge Ltd. - A Siemens Company
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|