TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, John Berg <[log in to unmask]>
Date:
Tue, 28 Feb 2006 13:01:33 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Schaefer, Chris" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Schaefer, Chris" <[log in to unmask]>
Parts/Attachments:
text/plain (74 lines)
Section 6.3.1 speaks about a 50% vertical hole fill on sections of the board that are considered thermal planes or conductor planes. It sounds like this applies, but it may require something from your customer to allow this or for reasons of stress it is required - not sure. We have issues such as your and we have spoken with the customer and have received the ok to allow a 50% fill versus the traditional 75%.

I agree with the previous point, but it will not allow for any process anomalies that occur on occasion. If for some reason the connector has issues related to the solderability, then you have a problem. In another scenario if the area/ connector has not been proper fluxed or achieved proper solder contact - it might look fine on the outside, but has not achieved the solderability levels you desire.

Food for thought...

Have a nice day guys!

Chris Schaefer
Suntron Corporation
Process Engineer
540 N. Rogers Road
Olathe, Kansas 66062
913.393.5878
[log in to unmask] 

NOTICE:
 
This message is intended for the use of the individual entity to which it is addressed and may contain information that is privileged, confidential and exempt from disclosure under applicable law. If the reader of this message is not the intended recipient, or the employee or agent responsible for delivering the message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by calling 913.393.5878 or returning the original message to us.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Berg
Sent: Tuesday, February 28, 2006 12:44 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Joint Inspection


If x-ray is not an option, you need to set up a soldering process that would not require inspection. On a thermally relieved pad that does not get sufficient fill, you need to preheat the pad area prior to hand soldering to compensate for the heat sinking. If you can get a dummy populated board, preheat it to a known reference level, and then remove the connector body to examine the % fill. Find the minimum reference preheat that will obtain your desired % fill. If you can't get a dummy populated board, you can use a few production boards to find the reference preheat by utilizing an ouitside x-ray service to determine the % fill.

>>> [log in to unmask] 2/28/2006 7:55 AM >>>
We are having a heck of a time inspecting some solder joints and could
use your help.

Per Class 3 a solder joint is supposed to have at least a 75% fill. We
have a circuit board that has large ground planes and hand soldered
connectors that are impossible to inspect for top side solder.

We do not have access to an x-ray and are wondering if there are any
clever ways to inspect these solder joints.

Thanks,

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2