Hann,
With respect to LTCC (Low Temp Co-fired Ceramic Packages) you could look at
the CTS web site at http://www.ctscorp.com/wireless/ffhome.htm for some
general info, or go to http://www.ctscorp.com/ffsearch.htm, type "ltcc AND
design AND guide" into the search window, open the cited document, then view
the design guide (Adobe format)
Steven Creswick - Gentex Corp
-----Original Message-----
From: Hann Pang [mailto:[log in to unmask]]
Sent: Monday, April 02, 2001 1:02 PM
To: [log in to unmask]
Subject: [TN] Moisture sensitivity
Experts!!
I'm helping a counterpart ask a few questions and i hope someone ,
somewhere might be able to help.
1) Where might someone go for information on ceramic packages? (LTCC)
2a) How are moisture sensitive finished ICs packages usually transported?
(tape and reel?)
2b) Do people use some sort of a moisture/water indicator (tape or any
other form)? if so, where/who can i get some samples from?
Regards,
Hann
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|