TECHNET Archives

May 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 25 May 2012 12:42:39 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="UTF-8"
Content-Transfer-Encoding:
quoted-printable
From:
Parts/Attachments:
text/plain (6 lines)
Low - P gives the fabricator less margin for error, the assembler, more margin.  Hgih P is the opposite.  But the margin on low P is VERY thin.    The change to mid-P is a big reason why black pad has become far less prevalent.  I would not accept <7% anymore

Higher P causes a near self limiting gold corrosion, keeping the gold from corroding the Nickel (black pad).  But it does concentrate the P near the Ni/Sn Intermetallic formation of the joint, making dark line defects (brittle P layer) easier to create during reflow.  High P also allows thinner gold, less to dissolve into the IMC.

Pete