Ken
Contrary to Brian's comments, Coating can SAVE your business
Save: Because you will have fewer field failures
Save: Because field failure could very well put you out of business
Save: Because if you design for coating, the cost is minimal v the benefit
Save: Because you may be compelled, by law, to coat - now why do you suppose
that is a mandate?
Save lives! - Circuits that are safety critical such as ABS, Air Bag or
Avionics systems, or weapons systems - where did my nuclear missile go? How
about utilities such as gas, electricity and water meters that often have to
survive for 20 years - GUARANTEED!
I might also point out - and others will correct me if I am wrong but - an
automobile could be guaranteed for more than 10 years if only the
electronics systems would last that long.
Come on Brian - your comments are not entirely fair. It is true to say,
no-one wants to coat but it need not be such a painful experience - what
price safety? Is $0.05 per assembly a high price to pay? - Play-station, TV,
Mobile phone, Computer OK, don't coat, after all, they would prefer you to
replace the unit.
I hope this helps you Ken but if you would like more, let me know
Regards
Graham Naisbitt
[log in to unmask]
Web: www.concoat.co.uk
Concoat Ltd
Alasan House, Albany Park
CAMBERLEY GU16 7PH
Tel: +44 (0) 1276 691100
Fax: +44 (0) 1276 691227
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ken Patel
Sent: Saturday, December 16, 2000 01:29
To: [log in to unmask]
Subject: [TN] Conformal Coating...
Guys,
What are the pros and cons of Conformal Coating on PWAs? Who are vendors in
San Jose Bay area?
re,
ken patel
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|