I am not party to the HP secrets for successful assembly with through hole
via in pad. I can say we tried pre-filling them with solder here and it did
not help.
The condition is a function of hole size, wetting forces, gravity, surface
tension, and reflow profile.
We have done it successfully, the problem is the hole must be quite small
and the aspect ratio of the PTH becomes difficult to produce if the boards
are a standard thickness.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ryan Grant
Sent: Tuesday, February 05, 2008 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] Open via in pad - any success?
Thanks Paul,
If you and two others can do it, I guess it can be done... I'm glad I
asked before I made a fool out of myself.
So now the question is, how did you do it (if you can tell me)?
Whenever I've tried it, either gravity would cause the solder to sag out
the bottom, or the via would suck solder away from the joint.
Thanks,
Ryan
________________________________
From: Paul Edwards [mailto:[log in to unmask]]
Sent: Monday, February 04, 2008 6:43 PM
To: TechNet E-Mail Forum; rgrant
Subject: RE: Open via in pad - any success?
Ryan,
It really depends on the size and depth of the via, the via to pad
diameter ratio....
Q: has anyone been successful with a via in pad that is not plugged?..
A: YES, both through and blind vias
Q: If so, was it double sided?
A: YES if you mean a double sided PCB, and YES if you mean it was a
through via..
Q: ...was one side connected to a BGA ball?
A: YES
Paul
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ryan Grant
Sent: Monday, February 04, 2008 4:55 PM
To: [log in to unmask]
Subject: [TN] Open via in pad - any success?
Hi All,
I just got told by a design engineer that LaserJet printers are built
using via in pad where the via is NOT plugged. He claims the via is
filled with solder first, then goes through the normal SMT process.
He intends to use this to connect a BGA ball on one side of the board to
a cap on the other side using an mechanically drill via that is not
plugged.
Before I call BS on this, and tell him "do not pass go until that via is
plugged, flattened and plated over", has anyone been successful with a
via in pad that is not plugged?
If so, was it double sided?
And, was one side connected to a BGA ball?
Thanks,
Ryan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
________________________________
This email and any attachments thereto may contain private,
confidential, and privileged material for the sole use of the intended
recipient. Any review, copying, or distribution of this email (or any
attachments thereto) by others is strictly prohibited. If you are not
the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this
email and any attachments thereto.
________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|