TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 3 Jun 2009 17:10:04 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Joe Fjelstad <[log in to unmask]>
Parts/Attachments:
text/plain (112 lines)
Hi Bob, 
 
I recall several folks making such comments over time on this forum an  
elsewhere. I have personally attempted refrained from making sweeping  
statements but I know folks out there with very strong  opinions. I like flying on 
Boeing planes because I once worked for  Boeing and know the quality of the 
plane and the evaluation systems (in general)  but I fly Airbus when that is 
the equipment being used knowing that I am not  going to live forever, nor 
am I going to live in blind  fear either.     
 
I note that Doug added a comment that is important. The military and  
aerospace are exempt but the suppliers of the component they use are not  and 
they are not interested in carrying two inventories for part numbers. 
 
There has been much discussion about the compatibility (or lack  thereof)  
of tin-lead and lead-free. Werner has mentioned how trying  to solve the 
problem by reballing may well be taking reliability in  the opposite direction 
due to the additional high temperature thermal  cycles. And tin whiskers? I 
note that there are new conferences that are  focusing on this topic. The 
list goes on... 
 
It is a thorny problem that seems not to have any clean resolution, save,  
perhaps, a return to the sanity of science based decision making relative to 
 electronics manufacturing rather than hasty emotional,  poorly thought out 
reasons from self serving politicians. 
 
So it goes...
 
Best wishes
Joe      
 
 
In a message dated 6/3/2009 10:56:34 A.M. Pacific Daylight Time,  
[log in to unmask] writes:

Joe,  several years ago, at PCB West, I attended a session which I
believe was a  panel discussion on RoHS topics.  A comment was made at
that time  about the new Airbus being certified as lead-free and one of
the panel  members made the observation that as long as that was the
case, he'd never  get on board an Airbus.  You were on that panel, and I
was just  curious if you remember that.   


Bob

-----Original  Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe  Fjelstad
Sent: Wednesday, June 03, 2009 12:38 PM
To:  [log in to unmask]
Subject: Re: [TN] Test

Thanks Steve


This  was both sad  event and very sobering. 


I recall hearing a few  years back of data being presented  indicating
that shock and  vibration resistance goes down for lead-free solders
over time with use.  

Has this been repeated, verified or seen by anyone else?  

Joe


**************Shop Inspiron, Studio and XPS Laptops at  Dell.com
(http://pr.atwola.com/promoclk/100126575x1222616459x1201464730/aol?redir
=http:%2F%2Fad.d
oubleclick.net%2Fclk%3B215218145%3B37264238%3Bd)

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery  of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To  receive ONE mailing per day of all the
posts: send e-mail to  [log in to unmask]: SET Technet Digest Search the
archives of previous posts  at: http://listserv.ipc.org/archives Please
visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional  information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100  ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------

**************Shop Inspiron, Studio and XPS Laptops at Dell.com 
(http://pr.atwola.com/promoclk/100126575x1222616459x1201464730/aol?redir=http:%2F%2Fad.d
oubleclick.net%2Fclk%3B215218145%3B37264238%3Bd)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2