Hello all,
Just a quick note for reference. The MicroBGA® CSP was designed to obviate
concern over the solder joint as a compliant element. In the µBGA® CSP, the
compliant layer in the package absorbs most of the stain of CTE mismatch
between silicon and FR-4 substate. As a result, the solder ball metallurgy
is not a great concern beyond allowing a good joint to be easily and
reliably formed in the assembly process and have sufficent strength to hold
fast the component in use.
Kind regards,
J. Fjelstad
At 12:41 AM 3/30/99 -0800, you wrote:
> Hi, Guenter, Werner...
> An opinion within the group of "leading lights" of UK technology,
> claim that "the lead free legislation is good timing" as Sn/Pb alloys
> do not have the reliability of other alloys, particularly with regard
> to modern components such as CSPs and Micro BGA.
>
> I have always understood that Pb makes Sn/Pb alloys very plastic and
> thus extreemly reliable under the stresses of thermal cycling.
>
> If there are more reliable alloys, what might they be?
> Which alloys present us with a higher degree of plasticity?
>
> Regards
> Edward Brunker
> PSION Computers
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|