Sender: |
|
X-To: |
|
Date: |
Mon, 18 Feb 2008 08:42:32 -0600 |
Content-Disposition: |
inline |
Reply-To: |
|
Content-Transfer-Encoding: |
7bit |
Subject: |
|
From: |
|
X-cc: |
|
In-Reply-To: |
<3B60FEB37FDB441E936E452AB5E9E9BD@StephenPC> |
Content-Type: |
text/plain; charset=ISO-8859-1 |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
ahhhh, thank you!
If I coulda remembered the word "patina" I coulda googled it myself.
I was just thinking of a brown penny, but now I have choices?
greenish?
blackish?
fun fun fun!
thanks again,
J
On 2/16/08, stephengregory5849 <[log in to unmask]> wrote:
>
> Hi Jack!
>
> Here's something I found:
>
> Green Patina Formula:
>
> 2 parts
> white vinegar
> 1 1/2 parts
> non-detergent ammonia
>
> 1/2 part
> non-iodized salt
>
>
> Application:
> a.. Clean fixture with Windex-type cleaner.
>
> b.. Premix patina solution in Windex-type spray bottle
> c.. Spray Windex cleaner on fixture to break surface tension,
> leaving it on when you apply patina solution.
> d.. Apply patina solution by spraying onto fixture, preferably in
> the early evening on a high humidity night.
> e.. Allow to set for 1 hour, then reapply solution observing where
> you missed applying on the first coat. If there seems to be oil that is
> repelling the patina solution, clean it off with the Windex cleaner.
> f.. Allow to sit overnight. In low humidity desert areas, use a
> plastic bag to create a tent over fixture (without making contact with it)
> to help keep the humidity high during curing. If there is low moisture in
> the air, the solution will dry out without creating the patina effect.
> g.. The result will be a bright green powdery patina. Do not rub
> off. In time (and re-applications) this finish will become permanent. The
> brightness will fade with time. To reduce green, cut back on the salt
> content. Color and effect is greatly affected by application ambient
> temperature and humidity.
> back to top
>
> Darkening Copper & Brass (penny brown):
> Brown Patina Formula
> Hot Water
> Baking Soda
> Place the hot water in a bottle. Add enough baking soda until it will
> not dissolve anymore when shaking the bottle.
>
> Application:
> Same as Green Patina. This finish is not as powdery and will not need
> as many re-applications
>
>
> Steve
>
> ----- Original Message -----
> From: "Jack Olson" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Saturday, February 16, 2008 12:30 PM
> Subject: [TN] NTC: Tarnishing Copper
>
>
> > Does anyone know how to make copper tarnish FASTER?
> >
> > (I want to make a wire sculpture look older)
> >
> > Saturday project.... Jack
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 15.0
> > To unsubscribe, send a message to [log in to unmask] with following text
> in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> > Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> > for additional information, or contact Keach Sasamori at [log in to unmask]
> > 847-615-7100 ext.2815
> > -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|