TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Pete menuez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Pete menuez <[log in to unmask]>
Date:
Mon, 25 Apr 2005 11:49:44 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Rob,
You may find the board shop very reluctant to process through concentrated
sulphuric acid. Plasma is the way to go.

You should require the board shop or the plasma service bureau to do a cross
section to evaluate etchback.  If they just stick your panels into a
"standard" etchback cycle there may be attributes on your panel that will
not plasma etch properly.  (Number of holes, diameter of holes, copper
weights etc>)

Also keep in mind plasma may not be even across the entire panel.

Good luck,

pete


>From: Robert Coburn <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
>[log in to unmask]
>To: [log in to unmask]
>Subject: [TN] Concentrated Sulfuric etchback
>Date: Thu, 21 Apr 2005 08:55:21 -0400
>
>Hi T'Netters:
>
>One of our divisions has a design that requires positive etchback on a four
>layer PCB (FR4 resin system).
>The board shop that had previously provided these boards subcontracted to a
>Plasma service.
>The etchback does not meet requirements.
>
>Does anyone have a contact that can provide a concentrated Sulfuric acid,
>Ammonium Biflouride etchback?
>
>TIA,
>Regards,
>Rob
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2