My question was answered.  Thank you everyon for your responses.



-----Original Message-----
From: Scott Westheimer [mailto:[log in to unmask]]
Sent: Wednesday, May 28, 2003 10:52 AM
To: [log in to unmask]
Subject: Re: [TN] Bad laminate and warped board


David,

A multi layer PCB is made with core material or "C" stage and is bonded
together with prepreg or "B" stage. Laminate or core material is made up of
copper foil and epoxy coated glass. Prepreg is epoxy coated glass which is
semi cured and when but together with core material and place in a press
flow and bonds the layers together. During the lamination cycle the prepreg
becomes fully cured. Hope this answers your question
Scott B. Westheimer
Gul Technologies PTE
5709 Clarks Fork Drive
Raleigh, North Carolina 27616
Phone: (919)713-4358
Fax: (919)713-4358
Cell: (919)649-1510
Email: [log in to unmask]
http:///www.gultech.com
----- Original Message -----
From: "Dave Tremmel" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, May 28, 2003 11:25 AM
Subject: Re: [TN] Bad laminate and warped board


Hello,

Could someone please explain what the term 'prepreg' is.

Thank you,

David Tremmel



-----Original Message-----
From: Robert Tarzwell [mailto:[log in to unmask]]
Sent: Tuesday, May 27, 2003 7:12 PM
To: [log in to unmask]
Subject: Re: [TN] Bad laminate and warped board


All very good therories but the reasons boards warp is many fold, usualy the
prepreg cant cause the problem unless many plies were layed ,or supplied
with the weave in the wrong direction, when you buy prepreg the weave
direction is printed on the vac bag. There are many places in a board shop
where warpage can be generated, The press cycle (too fast a cool down), the
press ( warped plates or plattens) The plating of unbalanced copper, the hot
air leveler, the ovens for solder mask, and white marking, the uv cure
machines , The biggest problem is not storing the boards in a flat position
when they are near or above the T/G the material is plastic like and easly
cures with a warp.
Can they be strightend, depends on the method used to warp them, If it is a
heat/bent in cooling problem yes a short cycle above the t/g and placed on a
flat surface with weights can return them to flat. but if it is a weave
problem no you can not permenitly strighten them. A quick test is to take a
board place it in a oven till the board is just above the T/G and take it
out and lay it on a flat surface with no weight, if the board goes flat it
was probably a handling issue, if its still bend then throw it out.
Long winded I know.
the major problem with a oven cycle to strighten the boards, is when you go
above the T/G  you only get so many of them. each transition above T/G
removes one solder cycle the assembler can do before cracking in the vias.
As a pcb manufacture knows after 4-6 solder floates you get via cracking!!
I think you need to talk with the manufacture and let him know warped boards
above the IPC standard will not be accepted.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2