Our laboratory measures this property near 10 GHz using the method described in MIL S 13949.
Please contact me if I can be of help.
Kuwako, Fujio(MMS) wrote:
> Is anybody know the test laboratory who can measure dielectric
> constant and dissipation factor of pwb material up to GHz?
>
> Kuwako
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################
--
John Moylan
President
Delsen Testing Laboratories, Inc.
1024 Grand Central Ave.
Glendale, CA 91201
Phone: 818 247 4106
FAX 818 247 4537
email: [log in to unmask]
URL: http://www.primenet.com/~delsen/
Delsen Testing Laboratories, Inc. is an independent testing
laboratory primarily engaged testing advanced materials.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|