TECHNET Archives

June 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Fri, 29 Jun 2007 09:47:12 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
A<7DF33F3ED1134D029AF8D36326CBC2C4@SteveKellyLap>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (68 lines)
Part of me wants to say that is shear lunacy.
 I would suggest reflowing solder balls to the pads and due a pull/shear
test. There are several test reports and Equipment people that could
help you with this. The goal would be to have a cohesive failure of the
solder ball. All that does is establish, regardless of the undefined
anomaly, that an acceptable adhesion can be attained at the ball/pad
interface.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly
Sent: Friday, June 29, 2007 7:42 AM
To: [log in to unmask]
Subject: [TN]

Good Morning to All,

I have a customer who has asked me to do an on-going test for black pad.
The
test would require me to solder wires onto 624 BGA pads and then pull on
the
wires to determine if there is black pad . They have given me no
criteria in
terms of pull strength or what constitutes pass/fail. I obviously need
some
kind of pull tester to do this. Has anyone done anything similar? Any
thoughts or ideas would be appreciated. Regards Steve Kelly

 

Steve Kelly

(416) 750-8433 (work)

(416) 750-0016 (fax)

(416) 577-8433 (cell)

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2