TECHNET Archives

July 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Charles Barker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 28 Jul 1999 12:51:22 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (83 lines)
OK, guys and gals,

Lets keep the comments to the technical, not the mundane! We all suffer
from typos here and there!




Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to "Marion A. Graybeal" <[log in to unmask]>



 To:      [log in to unmask]

 cc:      (bcc: Charles Barker/US/I-O INC)



 Subject: Re: [TN] Freeze Spray and BGAs









Werner,

I see that you and Dan Quail attended the same school (potatoe).

Marion Graybeal
----- Original Message -----
From: Werner Engelmaier <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, July 28, 1999 10:07 AM
Subject: Re: [TN] Freeze Spray and BGAs


>Hi Darrelt,
>What happened to your BGA is pretty obvious. Just consider what is
physically
>happening when you hit iot with the freeze spray.
>You hit the BGA with the freeze spry from the top, I am sure. This quickly
>cools the top layer of the BGA, the rest of the BGA to a lesser degree.
That
>sets up differential thermal shrinking (the opposite of thermal expansion
on
>heating), which causes the BGA to warp like a potatoe chip with the top
>surface being concave. This puts tremendous tensile stresses on the solder
>joints, as well as on other parts in the BGA depending on construction. On
>top of which, the PCB does not cool very much at all (the BGA shields it
from
>the freeze spray) and sets up shear stresses between the BGA and the PCB.
>I would not at all be surprised if failure analysis shows fractured solder
>joints. likely in combination of soldering pads ripped out of the polymer
>matrix.
>
>Werner Engelmaier
>Engelmaier Associates, L.C.
>Electronic Packaging, Interconnection and Reliability Consulting
>7 Jasmine Run
>Ormond Beach, FL  32174  USA
>Phone: 904-437-8747, Fax: 904-437-8737
>E-mail: [log in to unmask], Website: www.engelmaier.com
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2