Many, many moons ago when I was doing custom LSI packaging, thin film
hybrids, and multilayer thick film hybrids, MIL-STD-883 methods 2010 and
2017 defined acceptance criteria for wire bonds.
Hope this helps.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guenter Grossmann
Sent: Wednesday, January 30, 2008 11:16 AM
To: [log in to unmask]
Subject: [TN] Wedge bonds
Hi all
Is there a standard specifying the shape of wedge bonds?
Guenter
_____________________________________________________
EMPA
Swiss Federal Laboratories for Materials Testing and Research Centre
for Reliability Guenter Grossmann, Senior Engineer
8600 Duebendorf
Switzerland
Phone: xx41 44 823 4279
Fax : xx41 44 823 4054
mail: [log in to unmask]
_____________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|