TECHNET Archives

September 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"lduso - Diamond-MT.com" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, lduso - Diamond-MT.com
Date:
Thu, 3 Sep 2015 10:55:38 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (86 lines)
That sounds more like the problem, masking technique. We mask hundreds a
day and rarely damage anything. It's all in using the right technique and
as Steve said, the right material.

What coating are you using?

Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com

On Thu, Sep 3, 2015 at 10:43 AM, Adrian Dimulescu <[log in to unmask]>
wrote:

> That’s what we’re doing now, the issue is removing the mask as it will
> occasionally lift a pad or component.  We’re looking to do away with
> masking.
>
>
>
> Thanks
>
>
>
> ------------------------------
> *Adrian Dimulescu | Advanced Engineer | MtronPTI (NYSE MKT: LGL)*
> 2525 Shader Rd, Orlando, FL 32804
> Office: 407.298.2000
>
>
>
> *From:* lduso - Diamond-MT.com [mailto:[log in to unmask]]
> *Sent:* Thursday, September 03, 2015 10:41 AM
> *To:* TechNet E-Mail Forum; Adrian Dimulescu
> *Subject:* Re: [TN] Selective Conformal Coat Systems
>
>
>
> That low a volume, mask and spray by hand.
>
>
> Lloyd Duso
>
> Diamond-MT
> Plant Manager
> (814) 535-3505
>
> www.Diamond-mt.com
>
>
>
> On Thu, Sep 3, 2015 at 10:39 AM, Adrian Dimulescu <[log in to unmask]>
> wrote:
>
> Hello All,
>
> We're looking into purchasing a small (bench-top type) automated selective
> conformal coat system.  This will be used for 100 or so boards a week,
> therefore speed is not an issue.  It is important that the system is
> selective as we only want to coat specific areas on the board.  I wanted to
> get a feel for what other are using and/or recommend.
>
> Many Thanks
>
>
>
> CONFIDENTIALITY NOTICE:
> This email together with any attachments is confidential; intended for only the
> recipient(s) named above and may contain information that is privileged or
> exempt from disclosure under applicable law. If you have received this email in
> error, or are not the named recipient(s), you are hereby notified that any use,
> dissemination, distribution or copying of this email or any attachments is
> strictly prohibited. Please immediately notify the sender and delete this email
> and any attachments from your computer. You should not retain, copy or use this
> email or any attachments for any purpose, or disclose all or any part of the
> contents to any person.  The LGL Group, Inc. and its subsidiaries reserve the
> right to monitor all email communications through its networks.
>
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2