TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
John Burke <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 8 Jan 2007 09:58:59 -0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Burtt, Nigel" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Burtt, Nigel" <[log in to unmask]>
Parts/Attachments:
text/plain (109 lines)
Very common for SnPb solder paste over here to be the 2% silver loaded

variety ("brighter joints", slightly lower melt point at 179C, etc, etc)



________________________________



From: John Burke [mailto:[log in to unmask]] 

Sent: 05 January 2007 18:28

To: 'TechNet E-Mail Forum'; Burtt, Nigel

Subject: RE: [TN] Qualification of ROHS Components with tin/lead Solder







Interesting  - I note in the conclusions in the opening paragraph that

they state on the QFP failures:



" Failures in Sn-plated QFP components were probably due to batch

related solderability issues."



If you look at the "batch" you will find that this was:



4.3.5 QFP Electrical Testing

No electrical test failures occurred in any of the following

combinations:

- Batch A (SAC solder with SnPb QFPs)

- Batch B (SnPbAg solder with SnPb QFPs)

- Batch D (SnPbAg solder with Sn QFPs)

- Batches E2, E3, E4 and E5 (Contaminated solder with Sn QFPs)

Electrical failures occurred only in the following batch between 1000

and 2000 thermal

cycles

- Batch E1, 4 failures (SAC solder with Sn QFPs)





Since in any experiment of this sort all other variables are removed,

such as component batch, reflow profile, solder batch et al to avoid

skewing the results I draw the conclusion by looking at this data that

the "batch" they are referring to is actually a tin finish component

with SAC alloy combination, and that anyone using this combo is in for

an interesting time unless he is right in the "sweet spot" of a reflow

profile.





I find it extraordinary and very Interesting that they actually did not

use any 63/37 for the BGA trials (or any of the other testing given it's

market share historically) - I wonder why that would have been - anyone

know??







John









John Burke



(408) 515 4992



-----Original Message-----

From: TechNet [mailto:[log in to unmask] <mailto:[log in to unmask]> ] On

Behalf Of N Burtt

Sent: Friday, January 05, 2007 8:01 AM

To: [log in to unmask]

Subject: Re: [TN] Qualification of ROHS Components with tin/lead Solder



THE NPL project report



"Measuring the reliability of electronics assemblies during the

transition period to lead-free soldering."



can be downloded free at



http://tinyurl.com/t6vlt <http://tinyurl.com/t6vlt> 



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives

<http://listserv.ipc.org/archives>  Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16

<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>  for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------









-----------------------------------------

This message (including any attachments) may contain confidential
information intended for a specific individual and purpose.  If you
are not the intended recipient, delete this message.  If you are
not the intended recipient, disclosing, copying, distributing, or
taking any action based on this message is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2