Terry,
you have to find out what is the root cause of the open:
e.g. Drill smear or plating via thickness variation, etc.etc.
you may also experiences thermal expension abnormalty due to PWB stack
problem...etc.etc.
Based on your post, I don't believe your thermal stress simulated the
assembly condition (reflow or wave) extremes. Cross section of the problem
PWB area should help you a lot (start with X-ray if you have one).
my 1.3 cents. Good luck.
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Terry Exell
>Sent: Tuesday, July 16, 2002 2:46 AM
>To: [log in to unmask]
>Subject: [TN] Stress screening of multi layer production boards for
>optimum reliability
>
>
>Dear All,
>
>I am experiencing occasional open circuits on 16 layer boards
>during assembly and
>during in-service use. I have started thermal stressing all
>production boards with
>the aim of screening out any boards with latent defects and this
>is identifying and
>removing some problem boards. However, an equal number of problem
>boards still
>fail during assembly.
>
>Does anyone use similar thermal stressing of production boards to
>help improve
>assembly yields and product reliability? If so, do you find it successful?
>
>My thermal stressing uses the following parameters:
>10 cycles of hot / cold exposure in a HALT chamber,
>-60 deg C to +120 deg C temperature excursions,
>40 deg C per minute temperature ramp rate.
>The boards are electrically tested after thermal stressing.
>
>I calculate the screening is using approximately 20% of the
>expected life of the
>assembled boards, so I am reluctant to increase the stress levels.
>
>My board manufacturer has made several process improvements over
>the last year but
>I have not seen a significant improvement in my assembly yield.
>
>Best regards
>
>Terry Exell
>PCB Assembly Engineer
>BAE SYSTEMS
>Plymouth, UK
>
>
>
>********************************************************************
>This email and any attachments are confidential to the intended
>recipient and may also be privileged. If you are not the intended
>recipient please delete it from your system and notify the sender.
>You should not copy it or use it for any purpose nor disclose or
>distribute its contents to any other person.
>********************************************************************
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail
>to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|