TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 8 Mar 2006 07:15:26 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (71 lines)
Hi Guy! The use of Sn62 will slow down the leaching of the terminal but you
are still going to lose PdAg thickness. And you should be cautious on any
secondary soldering operations because you have the possibility of
completely leaching off the PdAg termination if you hand solder it a second
time (I have seen components fall off pwas). Does your customer have real
data demonstrating that a nickel or copper barrier layer on the capacitors
will cause a functional issue? The reason I ask is I once worked with a
program where the electrical engineers swore that the nickel barrier was
going to be a huge functional issue. When they started having capacitors
fall off the pwas (our soldering options were such that I couldn't
prevent/minimize the leaching actions) the equivalent capacitor with a
nickel barrier was used with no functional impact. Funny how real data
matters! Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




             Guy Ramsey
             <gramsey@RDCIRCUI
             TS.COM>                                                    To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             03/07/2006 01:35          [TN] soldering to PdAg cap
             PM


             Please respond to
             gramsey@rdcircuit
                   s.com






We are leaching the termination off of a capacitor. Our customer requires a
non-magnetic component and has specified a component without a nickel
barrier, because of nickel's ferromagnetic properties.
What can we do?


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2