TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Date:
Mon, 11 May 2009 17:35:18 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (150 lines)
Well thank a lot! I now have spittle all over my monitor....

Graham Naisbitt

On 11 May 2009, at 16:43, Whittaker, Dewey (EHCOE) wrote:

> So, since we are speaking of a vacuum deposition process, a Blonde was
> asked if she were in a vacuum, would she be able to hear. Is it on or
> off was her reply. May I please have a copy of that data?
> Dewey
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Tellefsen
> Sent: Monday, May 11, 2009 8:31 AM
> To: [log in to unmask]
> Subject: Re: [TN] Parylene Adhesion Tape Test
>
> Very silly response to unclear English.
>
> Paralene, when applied over some no-clean wave-soldering and solder
> paste
> flux residiues, does not provide good protection.
>
> I miss Al Schneider.
>
> Karen Tellefsen - Electrical Testing
> [log in to unmask]
> 908-791-3069
>
>
>
>
> So are you telling us not to use Al Schneider or no-clean soldering
> materials?
> Dewey
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Tellefsen
> Sent: Monday, May 11, 2009 6:34 AM
> To: [log in to unmask]
> Subject: Re: [TN] Parylene Adhesion Tape Test
>
> At Nepcon west 1999, Al Schneider presented some work  I did on  
> Paralene
> and no-clean soldering  materials with disappointing results.  If  
> anyone
> wants a copy, email me.
>
> Karen Tellefsen - Electrical Testing
> [log in to unmask]
> 908-791-3069
>
>
>
>
>
>             Mary Lou Sachenik
>
>
>
>
> Subject
>             05/09/2009 07:59          [TN] Parylene Adhesion Tape Test
>
>             AM
>
>
>
>
>
>             Please respond to
>
>              TechNet E-Mail
>
>                   Forum
>
>             <[log in to unmask]>
>
>
>                    OM>
>
>
>
>
>
>
>
>
>
> We recently had some issues with lack of adhesion of Parylene coating
>
> What types of notes are being used on drawings to define parylene
> conformal coating adhesion test on pwa's?
> Is the ASTM3359-08 (for assessing the adhesion of coating films to
> metallic substrates) the best spec to call out for this testing .
> I presently don't have pwb coupons to perform destructive cross hatch
> test.
>
> What type of tape is being used testing parylene adhesion on the  
> PWA's?
> Some specs call out 3M-250 tape, the ASTM D 3359 calls out the  
> Permacel
> 99.
> Actually I prefer the Wescorp 79210 clear Anti-static Tape, does this
> seem
> acceptable?
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or  
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following  
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask] 
> : SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask] 
> : SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
>  for additional information, or contact Keach Sasamori at [log in to unmask] 
>  or 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2